Economical Anticorrosive Chlorinated Rubber Based Primer Supplier in China
Economical Anticorrosive Chlorinated Rubber Based Primer paint coating manufacture Shenzhen China  
Home About Us Products Contact Us

 

 




Honest Joy Coating & Paint
Vinyl Coating

Chemical Resistant Chlorinated Rubber Based Enamel
Chlorinated Rubber Based Anti-corrosive Primer
Chlorinated Rubber Swimming Pool Paint
Chlorinated Rubber Enamel

Chlorinated Rubber High Build Coating
Economical Anticorrosive Chlorinated Rubber Based Primer
Tintable Chlorinated Rubber Finish
Polychloroprene Rubber Solvent Based Primer
Phisically Drying Modified Chlorinated Rubber Based Primer
General Purpose Chlorinated Rubber Primer
Chlorinated Rubber Intermediate Coating

Chlorinated Rubber Micaceous Iron Oxide coating
Premium Quality Full-bodied Smooth-flowing Vinyl-acrylic Primer
Abrasion Resistant Vinyl Ester Coating
Catalyzed Vinyl Ester Primer
Chlorinated Rubber Based Intermediate Coat

Chlorinated Rubber MIO Intermediate Coating

  

Economical Anticorrosive Chlorinated Rubber Based Primer

PRODUCT SPECIFICATIONS:

DESCRIPTION
An economical anticorrosive chlorinated rubber based primer for interior/exterior protection of metal substrates. It provides good chemical and moisture resistance with superior adhesion to various metal substrates.
RECOMMENDED USES
For use over prepared steel, iron, aluminum, galvanized metal, paper plant, and laundries.
CHARACTISTICS
Color:
Red Brown
Finish:
Matt
Volume Solid:
36% +1%
Specific Gravity:
1.50 KGs / ltr
Recommended DFT:
75 Microns
Spreading Rate@DFT:
4.80 m2 / ltr or
18. m2 / gallon
Flash Point:
26 C
Drying Schedule:
@ 25 oC/R.H.50
Dry to Touch:
15 Minutes
To Handle:
2 Hours
To Recoat:
1 Hours
Shelf Life:
18 months, unopened at 25 oC
Reducer/Clean Up:
Industrial thinner HJ-376
APPLICATION PROCEDURES
Surface Preparation:Surface must be dry, clean and in sound condition. Remove oil, dust, dirt, millscale or other foreign substance to ensure good adhesion. Minimum surface preparation methods to be followed for (1) Iron and Steel – SSPC-SP2 or SP3 (2) Aluminum and Galvanizing – SSPC-SP1. Allow weathering of new galvanized steel for six months prior to coating.
Application Methods:
Conventional Spray:
Reduce 10% with industrial thinner
Airless Spray:
Reduce 10% with industrial thinner
Brush/Roller:
Reduction not recommended
SYSTEM RECOMMENDATION
Iron and Steel:
Hi-Build Chlorinated Primer
1 Coat
75 Microns DFT
Industrial Lacquer
Putty
1 Coat
150 Microns DFT
Recommended Topcoats
2 Coats
As Recommended
Aluminum and Galvanized Metal:
Wash Primer
1 Coat
07 Microns DFT
Hi-Build Chlorinated Primer
1 Coat
75 Microns DFT
Recommended
Topcoats
2 Coats
As Recommended
Topcoats Recommended:
• Hi-Build Chlorinated Rubber Enamel
• Sheracryl Acrylic Enamel (Gloss, Semigloss, Flat, Clear)
• Alkyd Enamels (Gloss, Semigloss, Flat)
• Hi-Build Aliphatic Polyurethane
• Epoxy


SAFETY PRECAUTIONS
Spray under well-ventilated conditions. Do not breathe or inhale mist. When spraying, wear air mask. Avoid skin contact. Spillage on skin should immediately be removed with suitable cleanser, soap and water. Eyes should be flushed with water and medical attention sought immediately.

 

 



Contact Us
 
Honest Joy Coating & Paint. All rights reserved.